In Vivo Stability of Polyurethane-Based Electrospun Vascular Grafts in Terms of Chemistry and Mechanics Научная публикация

Журнал Polymers
ISSN: 2073-4360
Вых. Данные Год: 2020, Том: 12, Номер: 4, Номер статьи : 845, Страниц : DOI: 10.3390/polym12040845
Ключевые слова tecoflex; pellethane; gelatin; electrospinning; vascular grafts; polyurethane stability in vivo
Авторы Gostev Alexander A. 1 , Shundrina Inna K. 2,3 , Pastukhov Vitaliy I. 2,3 , Shutov Alexey V. 3,5 , Chernonosova Vera S. 4 , Karpenko Andrey A. 1 , Laktionov Pavel P. 1,4
Организации
1 (Данные Web of science) Minist Hlth Russian Federat, Meshalkin Natl Med Res Ctr, Novosibirsk 630055, Russia
2 (Данные Web of science) Russian Acad Sci, Siberian Branch, Vorozhtsov Novosibirsk Inst Organ Chem, Novosibirsk 630090, Russia
3 (Данные Web of science) Novosibirsk State Univ, Ul Pirogova 2, Novosibirsk 630090, Russia
4 (Данные Web of science) Russian Acad Sci, Siberian Branch, Inst Chem Biol & Fundamental Med, Novosibirsk 630090, Russia
5 (Данные Web of science) Russian Acad Sci, Siberian Branch, Lavrentiev Inst Hydrodynam, Novosibirsk 630090, Russia

Реферат: The biostability of the polyurethanes Tecoflex EG-80A and Pellethane 2363-80A, used as basic polymers of the vascular grafts (VGs) produced by electrospinning, as well as the tensile strength of Tecoflex VGs, are studied. Solutions of Tecoflex or Pellethane with gelatin and bivalirudin in 1,1,1,3,3,3-hexafluoroisopropanol are used for VG production. After 1, 12, and 24 weeks of VG implantation in the infrarenal position of the abdominal aorta of Wistar rats, VGs are explanted, fixed in formalin, freed from outer tissues, dialyzed, and dried. The polyurethanes are extracted from VGs by dispersion/extraction in tetrahydrofuran (THF) and freed from the excess of THF-insoluble biopolymers. The stability of polyurethanes is assessed by IR spectroscopy and gel permeation chromatography. Pellethane has emerged to be stable at all experimental points. Tecoflex loses approximately 10% of its molecular weight (both M-n and M-w) after 3 months and restored its initial value within 6 months of its functioning as a graft. Mechanical testing demonstrates a 30% reduction in the tensile strength after 3 months in VG and a 10% increase after 6 months. The stability and mechanical properties of polyurethane-based VGs demonstrate their utility for the reconstitution of damaged arteries.
Библиографическая ссылка: Gostev A.A. , Shundrina I.K. , Pastukhov V.I. , Shutov A.V. , Chernonosova V.S. , Karpenko A.A. , Laktionov P.P.
In Vivo Stability of Polyurethane-Based Electrospun Vascular Grafts in Terms of Chemistry and Mechanics
Polymers. 2020. V.12. N4. 845 . DOI: 10.3390/polym12040845 WOS Scopus РИНЦ OpenAlex
Файлы: Полный текст от издателя
Даты:
Опубликована online: 7 апр. 2020 г.
Идентификаторы БД:
Web of science: WOS:000535587700115
Scopus: 2-s2.0-85086627614
РИНЦ: 43305984
OpenAlex: W3014554875
Цитирование в БД:
БД Цитирований
Web of science 18
Scopus 17
РИНЦ 18
OpenAlex 18
Альметрики: